> Right you are! One other thing, If you re heat after rolling and then 
> quickly dip in water it does re harden the metal! WNW has this method 
> described in their hints section on their builds.
> Rick G.

Ok, that's the final piece of the puzzle. I knew there was a dip it in 
water step somewhere.

Heat it, let it cool, roll on a soft surface, heat it again and dip it 
in water to anneal and harden it.